A research group in Japan identified a correlation between damp heat test of 1,000 hours to 3–6 years of field exposure in humid areas and changes in acetic acid concentration in photovoltaic modules.
A research team in Germany has investigated whether compressive stress relaxation measurement (CSRM) can be used to monitor polymer degradation in aging photovoltaic modules. The technique is ...